Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Premix Thermoplastics PREADD AB 172 PREADD AB 172 is a PE-LD based antiblock masterbatch developed for polyethylene films over 35µm in thickness.The addition of PREADD AB 172 gives following advantages to films:Increased heat conduct.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
NEXA® PFX8010 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Long Term |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | (Expected) Continuous use, UL |
Gharda Chemicals GATONE™ 5400 PEEK, Medium Viscosity Grade
(discontinued **) Medium viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical prope.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
Solvay Specialty Polymers Algoflon® 25CAR+5CER PTFE; Petroleum Coke and Ceramic Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke + 5 wt.% Ceramic. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectr.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Intermittent |
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® H7525 Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® SG03-06(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® SG26-06(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® SG36-06(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® SG36-10(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | UL-746 B |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.125" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® 2255-2 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® 2285-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | intermittent |
Thermoseal ML-N562 PTG Gasketing Thermoseal ML-N562 is a synthetic fiber and nitrile butadiene gasket material designed for difficult sealing applications with very low flange pressures or very rough surface finishes. It combines M.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Extended |
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
CoorsTek PolyGlyde™ 1000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous use |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Intermittent |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | retains useful mechanical properties |
Chemours Teflon® PTFE 612A Resin for Lubricated Paste Extrusion Available in white powder, often called "fine powder," this fluoropolymer resin is capable of being sheared by lubricated paste extrusion (facilitated by a hydrocarbon liquid) into a coherent fibrou.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | retains useful mechanical properties |
Chemours Teflon® PTFE 67 Resin for Lubricated Paste Extrusion Available in white powder, often called "fine powder," this fluoropolymer resin is capable of being sheared by lubricated paste extrusion (facilitated by a hydrocarbon liquid) into a coherent fibrou.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | continuously and up to 316°C (600°F) intermittently |
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C.. |