Material Notes:
Fluoroplastic THV is a flexible, fluoroplastic electrostatic dissipative compound composed of tetrafluoroethylene, hexafluoropropylene and vinylidene fluoride in the form of pellets.Information provided by 3M
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min
5.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F