Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | STN 34 6460 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | DIN 53482 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 116 N/L GPPS Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 156F GPPS Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 168 N/L GPPS Styrolution PS 168N/L is a high molecular weight, heat resistant grade with high mechanical strength. It is suitable for physically or chemically expanded extruded sheet. It is also suitable for use.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner PP430R Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON F-205 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Adamas Adalon® 998 PTFE, Turquoise Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | STN 34 6460 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |