Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN.52612 (dry sample)
Omnia Plastica Akulon® PA 66 - Akulon 66 - at 50% RH
Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN.52612 (dry sample)
Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH
Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data)
This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM D177
Manifattura Cattaneo PEEK Polyetheretherketone
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Thermal Conductivity >= 0.250 W/m-K
>= 1.74 BTU-in/hr-ft²-°F
ASTM C177
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber
The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional ..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1/GK/30/TF/13/SI/2 Polyamide 66, with glass spheres, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1105/RD7405 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry
Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Thermal Conductivity 0.250 W/m-K

@Temperature 121 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 250 °F
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive
TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Elisto THERMOSTAR® 600 n Mold Insulation Material
Insulation of clamping platesInformation provided by elisto
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON F-201 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into ..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder
30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM
High impact resistanceInformation provided by E-Polymers Co. Ltd.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Chemours Teflon® PTFE 7A Granular Molding Powder
Teflon® PTFE white granular molding powders are ideal for molding many different end products and stock shapes. Excellent chemical resistance, electrical properties, high temperature performance, ..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..