Material Notes:
Non-lead stabilized, 105°C rated insulation compound recommended for various style # applications including 1007 and 1015. The compound is formulated for microbial and fungal resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 94
88 - 94
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 267.5 %
267.5 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
320 %
320 %
ASTM D-638
100% Modulus 0.01169 GPa
1.695 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -23.0 °C
-9.40 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+14 ohm-cm
9.00e+14 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F