Material Notes:
Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydrolytic stability, oil, fuel and solvent resistance. It is supplied uncolored in pellet form. Availability: North AmericaFeatures: Fuel Resistant, Good Toughness, Oil Resistant, Hydrolytically Stable, Solvent Resistant, Good Abrasion Resistance Appearance: ColorlessForms: PelletsProcessing Method: Injection MoldingInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D412
Tensile Stress 12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D412
18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Tear Strength 75.0 kN/m
428 pli
Die C; ASTM D412
Taber Abrasion, mg/1000 Cycles 35
35
ASTM D1044
Abrasion 28
28
mm<sup>3</sup>; DIN 53516
Compression Set 20 %

@Temperature 22.8 °C,
Time 79200 sec
20 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D3995B
35 %

@Temperature 70.0 °C,
Time 259000 sec
35 %

@Temperature 158 °F,
Time 72.0 hour
ASTM D3995B
Thermal Properties Metric English Comments
Vicat Softening Point 75.0 °C
167 °F
ASTM D1525
Brittleness Temperature 18.4 °C
65.2 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Processing Temperature 190 - 195 °C
374 - 383 °F
Injection
Rear Barrel Temperature 165 °C
329 °F
Injection
Middle Barrel Temperature 180 °C
356 °F
Injection
Front Barrel Temperature 195 °C
383 °F
Injection
Nozzle Temperature 195 - 200 °C
383 - 392 °F
Injection
Mold Temperature 25.0 - 60.0 °C
77.0 - 140 °F
Injection
Injection Velocity >= 10.0 mm/sec
>= 0.394 in/sec
Injection
Drying Temperature 85.0 °C
185 °F
Injection
Dry Time 4.00 hour
4.00 hour
Injection
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection