Processing Properties Metric English Comments
Processing Temperature 190 - 230 °C
374 - 446 °F
PolyChem Alloy PolyFoam DC5
PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph..
Processing Temperature 190 - 265 °C
374 - 509 °F
Cylinder temp
Techno Polymer Techno ABS LM100 Transparent
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Processing Temperature 190 - 240 °C
374 - 464 °F
IRPC Polimaxx Polene 2300SC Polypropylene Block Copolymer
CHARACTERISTICS: HIGH FLOW, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, THIN WALL PARTS
Processing Temperature 190 - 240 °C
374 - 464 °F
IRPC Polimaxx Polene 2363LC Polypropylene Block Copolymer
CHARACTERISTICS: CONTAIN UV STABILIZER ADDITIVE, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, FURNITURES, CRATES
Processing Temperature 190 - 220 °C
374 - 428 °F
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI..
Processing Temperature 190 - 260 °C
374 - 500 °F
IRPC Polimaxx Porene AP102 Acrylonitrile Butadiene Styrene
Applications:automotive componentsradiator grillsname platesknobstv componentscosmetic componentselectronic household appliances ectespecially suited for electroplating and painting articles
Processing Temperature 190 - 240 °C
374 - 464 °F
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene
Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys
Processing Temperature 190 °C
374 °F
Metering Temperature
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 190 - 200 °C
374 - 392 °F
C1
UBE 7024B Nylon 6/12 Copolymer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
Processing Temperature 190 - 250 °C
374 - 482 °F
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat..
Processing Temperature 190 - 210 °C
374 - 410 °F
DSM Biomedical CarboSil® 20 55D Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU)
A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th..
Processing Temperature 190 - 230 °C
374 - 446 °F
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Processing Temperature 190 - 220 °C
374 - 428 °F
Extrusion Range
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Processing Temperature 190 - 230 °C
374 - 446 °F
Injection
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 13031 XF POM, Specialty
Hostaform« acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fu..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological
POM copolymerInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® LW90EWX POM, Tribological
Hostaform« LW90EWX is a specialty low wear grade of acetal copolymer designed for improved performance including when paired against other thermoplastic resins (PBT, PA, PC, PMMA) or steel. Due to ..
Processing Temperature 190 - 200 °C
374 - 392 °F
hot runner
Celanese Hostaform® S 27063 POM, Impact Modified
Chemical abbreviation according to ISO 1043-1: POM-HI,Information provided by Celanese
Processing Temperature 190 - 200 °C
374 - 392 °F
hot runner
Celanese Hostaform® TF-10XAP® POM, Impact Modified
Hostaform« acetal copolymer TF-10 XAP« is low emission, improved flow, impact modified grade providing optimum performance in general purpose injection molding primarily for the interior automot..
Processing Temperature 190 - 200 °C
374 - 392 °F
hot runner
Celanese Celcon® CF802 POM, Specialty
Celcon« acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon« CF802 has been developed to dissipate static electricity from fuel handling systems...
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 27021 POM, Unfilled
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® M25AE POM, Unfilled
Hostaform« M25AE is a special grade of acetal copolymer targeted for extrusion shapes (rod, bar, plate, etc) free of center porosity in large diameters and thicknesses.Information provided by Celan..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® XGC15-LW01 POM, 15% Glass Reinforced
Hostaform« XGC15-LW01 is an injection molding grade reinforced with approx. 15% glass fibers and tribological modification for sliding applications requiring low friction and wear.Information provi..
Processing Temperature 190 - 290 °C
374 - 554 °F
Average value: 223 °C Grade Count:25
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 13021 RM POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 13031 XAP POM, Unfilled
Polyacetal copolymer, reduced emissionInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 AW XAP² ™ LS POM, Tribological
POM copolymerInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 210 °C
374 - 410 °F
hot runner
Celanese Hostaform® C 9021 GV1/30 GT POM, 26% Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Processing Temperature 190 - 200 °C
374 - 392 °F
hot runner
Celanese Celcon® MC270 POM, Mineral Reinforced
Celcon« MC270 is a mineral coupled acetal copolymer designed for applications requiring improved stiffness, lower mold shrinkage and reduced warpage while maintaining the mechanical performance cha..