Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | [Mpa/cm<sup>2</sup>] |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Clamp Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | [Mpa/cm<sup>2</sup>] |
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Clamp Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | [Mpa/cm<sup>2</sup>] |
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |