Polymer Property : Tear Strength = 75.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 75.0 kN/m
>= 428 pli
Method B; ISO 34
S&E Specialty Polymers XP23-45MG PVC
Description: PVC weatherable, integral colored, filledApplication: Body side molding end caps and extruded skin compound which meets Chrysler MSDC 543 and Ford WSK-M4D689-A3Information provided by ..
Tear Strength 75.0 kN/m
428 pli
Die C, 2 in/min; ASTM D1004
PolyOne Geon™ Vinyl Flexible 90059 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tear Strength 75.0 kN/m
428 pli
100 micron film; ASTM D1004
Kaneka PHBH Semi-Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 75.0 kN/m
428 pli
DIN 53515
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 75.0 kN/m
428 pli
DIN 53515
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 75.0 kN/m
428 pli
without incision; ISO 34B
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 75.0 kN/m
428 pli
with incision; ISO 34B
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
Tear Strength 75.0 kN/m
428 pli
GB/T 529
Chengdu Polyster 9500 General Grade TPV
Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 75.0 kN/m
428 pli
DIN ISO 34-1/Bb
BASF Elastollan 685 AU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tear Strength 75.0 kN/m
428 pli
DIN ISO 34-1/Bb
BASF Elastollan C 88 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tear Strength 75.0 kN/m
428 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tear Strength 75.0 kN/m
428 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer
Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tear Strength 75.0 kN/m
428 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tear Strength >= 75.0 kN/m
>= 428 pli
ISO 34
Austin Novel Materials Texalan® 382A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tear Strength >= 75.0 kN/m
>= 428 pli
ISO 34
Austin Novel Materials Texalan® 485A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tear Strength 75.0 kN/m
428 pli
DIN ISO 34-1/Bb
BASF Elastollan B 85 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tear Strength 75.0 kN/m
428 pli
ISO 34-B
AlphaGary Evoprene™ HP 3732 High Performance Thermoplastic Elastomer
Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP..
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU
Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 75.0 kN/m
428 pli
Trouser Tear resistance TD; ISO 6383-1
EMS-Grivory Grivory® BM 20 SBG PA*
Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther..