Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 195 - 205 °C | 383 - 401 °F | |
Huntsman AVALON® 98 AE Thermoplastic Polyurethane Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Front Barrel Temperature | 195 - 215 °C | 383 - 419 °F | Injection Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 195 - 205 °C | 383 - 401 °F | |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Front Barrel Temperature | 195 - 205 °C | 383 - 401 °F | |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Front Barrel Temperature | 195 - 205 °C | 383 - 401 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Front Barrel Temperature | 195 - 205 °C | 383 - 401 °F | |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
Front Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Start Point: 210°C |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPU-E90 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPUI-E95 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPUI-H95 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Metering zone |
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Front Barrel Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Front Barrel Temperature | 195 °C | 383 °F | Injection |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |