Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 18.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 18.0 MPa

@Strain 50.0 %
2610 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..
Tensile Stress 18.0 MPa

@Strain 50.0 %
2610 psi

@Strain 50.0 %
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..
Tensile Stress 18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
Tensile Stress 18.0 MPa

@Strain 0.440 %,
Temperature 150 °C
2610 psi

@Strain 0.440 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
Tensile Stress 18.0 MPa

@Strain 0.150 %,
Temperature -40.0 °C
2610 psi

@Strain 0.150 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 18.0 MPa

@Strain 0.480 %,
Temperature 23.0 °C
2610 psi

@Strain 0.480 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer
Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 18.0 MPa

@Strain 200 %
2610 psi

@Strain 200 %
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress 18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Tensile Stress 18.0 MPa

@Strain 200 %
2610 psi

@Strain 200 %
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress 18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Tensile Stress >= 18.0 MPa

@Strain 300 %
>= 2610 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 490A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 18.0 MPa

@Strain 100 %
>= 2610 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 498A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 18.0 MPa

@Strain 100 %
>= 2610 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 664D Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 18.0 MPa

@Strain 10.0 %,
Time 3.60e+6 sec
2610 psi

@Strain 10.0 %,
Time 1000 hour
60°C; ISO 527
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
Copyright © lookpolymers.com All Rights Reserved