Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 1.40 g/cc
0.0325 - 0.0506 lb/in³
Average value: 1.07 g/cc Grade Count:7
Viscosity Test 100 - 200 cm³/g
100 - 200 cm³/g
Average value: 153 cm³/g Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Shore D 80.0 - 89.0
80.0 - 89.0
Average value: 82.8 Grade Count:4
Ball Indentation Hardness 108 - 200 MPa
15700 - 29000 psi
Average value: 132 MPa Grade Count:4
Tensile Strength, Ultimate 50.0 - 140 MPa
7250 - 20300 psi
Average value: 72.5 MPa Grade Count:4
Tensile Strength, Yield 60.0 - 98.0 MPa
8700 - 14200 psi
Average value: 72.5 MPa Grade Count:6
Elongation at Break 2.10 - 150 %
2.10 - 150 %
Average value: 88.1 % Grade Count:7
>= 50.0 %

@Temperature 80.0 - 80.0 °C
>= 50.0 %

@Temperature 176 - 176 °F
Average value: 50.0 % Grade Count:1
Elongation at Yield 3.00 - 9.00 %
3.00 - 9.00 %
Average value: 7.56 % Grade Count:6
Modulus of Elasticity 1.40 - 10.0 GPa
203 - 1450 ksi
Average value: 3.12 GPa Grade Count:6
1.27 - 1.27 GPa

@Temperature 80.0 - 80.0 °C
184 - 184 ksi

@Temperature 176 - 176 °F
Average value: 1.27 GPa Grade Count:1
Flexural Yield Strength 50.0 - 190 MPa
7250 - 27600 psi
Average value: 87.1 MPa Grade Count:4
Flexural Modulus 1.65 - 12.0 GPa
239 - 1740 ksi
Average value: 4.05 GPa Grade Count:5
Charpy Impact Unnotched 7.70 J/cm² - NB
36.6 ft-lb/in² - NB
Average value: 7.70 J/cm² Grade Count:5
5.90 J/cm² - NB

@Temperature -30.0 - 0.000 °C
28.1 ft-lb/in² - NB

@Temperature -22.0 - 32.0 °F
Average value: 6.45 J/cm² Grade Count:5
Charpy Impact, Notched 0.900 - 1.80 J/cm²
4.28 - 8.57 ft-lb/in²
Average value: 1.35 J/cm² Grade Count:6
0.600 - 1.70 J/cm²

@Temperature -30.0 - 0.000 °C
2.86 - 8.09 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 1.24 J/cm² Grade Count:6
Tensile Creep Modulus, 1 hour 1300 - 10000 MPa
189000 - 1.45e+6 psi
Average value: 4230 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 700 - 8300 MPa
102000 - 1.20e+6 psi
Average value: 3230 MPa Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 32.0 - 90.0 µm/m-°C
17.8 - 50.0 µin/in-°F
Average value: 67.0 µm/m-°C Grade Count:6
CTE, linear, Transverse to Flow 30.0 - 90.0 µm/m-°C
16.7 - 50.0 µin/in-°F
Average value: 75.0 µm/m-°C Grade Count:4
Melting Point 250 °C
482 °F
Average value: 250 °C Grade Count:3
Maximum Service Temperature, Air 100 °C
212 °F
Average value: 100 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 100 - 150 °C
212 - 302 °F
Average value: 123 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 93.0 - 140 °C
199 - 284 °F
Average value: 110 °C Grade Count:7
Vicat Softening Point 105 - 158 °C
221 - 316 °F
Average value: 134 °C Grade Count:6
Glass Transition Temp, Tg 108 - 150 °C
226 - 302 °F
Average value: 136 °C Grade Count:5
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:5
Glow Wire Test 850 °C
1560 °F
Average value: 850 °C Grade Count:3
Optical Properties Metric English Comments
Transmission, Visible 85.0 - 90.0 %
85.0 - 90.0 %
Average value: 89.2 % Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm
1.00e+15 - 1.00e+17 ohm-cm
Average value: 5.05e+16 ohm-cm Grade Count:6
Surface Resistance 1.00e+13 - 1.00e+15 ohm
1.00e+13 - 1.00e+15 ohm
Average value: 5.05e+14 ohm Grade Count:6
Dielectric Constant 3.00 - 5.00
3.00 - 5.00
Average value: 3.56 Grade Count:6
Dielectric Strength 21.0 - 35.0 kV/mm
533 - 889 kV/in
Average value: 27.5 kV/mm Grade Count:4
Dissipation Factor 0.0115 - 0.0325
0.0115 - 0.0325
Average value: 0.0217 Grade Count:6
Comparative Tracking Index 575 - 600 V
575 - 600 V
Average value: 589 V Grade Count:6