Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.16 - 1.82 g/cc
0.0419 - 0.0658 lb/in³
Average value: 1.45 g/cc Grade Count:136
Filler Content 10.0 - 50.0 %
10.0 - 50.0 %
Average value: 24.3 % Grade Count:21
Water Absorption 0.600 - 6.50 %
0.600 - 6.50 %
Average value: 1.79 % Grade Count:30
Moisture Absorption at Equilibrium 0.170 - 4.00 %
0.170 - 4.00 %
Average value: 1.53 % Grade Count:19
Water Absorption at Saturation 4.00 - 9.00 %
4.00 - 9.00 %
Average value: 5.20 % Grade Count:5
Additive Loading 20.0 - 50.0 %
20.0 - 50.0 %
Average value: 32.5 % Grade Count:4
Viscosity Test 104 - 150 cm³/g
104 - 150 cm³/g
Average value: 135 cm³/g Grade Count:4
Linear Mold Shrinkage 0.000800 - 0.0150 cm/cm
0.000800 - 0.0150 in/in
Average value: 0.00456 cm/cm Grade Count:120
Linear Mold Shrinkage, Transverse 0.00100 - 0.0158 cm/cm
0.00100 - 0.0158 in/in
Average value: 0.00839 cm/cm Grade Count:52
Melt Flow 1.00 - 55.0 g/10 min
1.00 - 55.0 g/10 min
Average value: 13.1 g/10 min Grade Count:32
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110 - 121
110 - 121
Average value: 118 Grade Count:20
Hardness, Shore D 80.0 - 90.0
80.0 - 90.0
Average value: 87.2 Grade Count:5
Ball Indentation Hardness 120 - 370 MPa
17400 - 53700 psi
Average value: 203 MPa Grade Count:9
Tensile Strength, Ultimate 30.0 - 210 MPa
4350 - 30500 psi
Average value: 116 MPa Grade Count:126
10.0 - 105 MPa

@Temperature 60.0 - 150 °C
1450 - 15200 psi

@Temperature 140 - 302 °F
Average value: 50.2 MPa Grade Count:6
Tensile Strength, Yield 50.0 - 210 MPa
7250 - 30500 psi
Average value: 111 MPa Grade Count:16
Elongation at Break 1.00 - 30.0 %
1.00 - 30.0 %
Average value: 3.73 % Grade Count:128
1.20 - 15.0 %

@Temperature 60.0 - 150 °C
1.20 - 15.0 %

@Temperature 140 - 302 °F
Average value: 6.45 % Grade Count:6
Elongation at Yield 2.00 - 9.70 %
2.00 - 9.70 %
Average value: 3.40 % Grade Count:12
1.70 - 4.50 %

@Temperature 90.0 - 150 °C
1.70 - 4.50 %

@Temperature 194 - 302 °F
Average value: 2.95 % Grade Count:2
Modulus of Elasticity 0.620 - 18.6 GPa
89.9 - 2700 ksi
Average value: 8.21 GPa Grade Count:95
1.70 - 7.80 GPa

@Temperature 60.0 - 150 °C
247 - 1130 ksi

@Temperature 140 - 302 °F
Average value: 4.22 GPa Grade Count:6
Flexural Yield Strength 73.6 - 310 MPa
10700 - 45000 psi
Average value: 179 MPa Grade Count:95
Flexural Modulus 1.10 - 17.9 GPa
160 - 2600 ksi
Average value: 7.09 GPa Grade Count:96
Compressive Yield Strength 75.8 - 103 MPa
11000 - 15000 psi
Average value: 94.8 MPa Grade Count:4
Izod Impact, Notched 0.280 - 1.80 J/cm
0.525 - 3.37 ft-lb/in
Average value: 0.941 J/cm Grade Count:45
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 7.47 J/cm Grade Count:19
Izod Impact, Notched (ISO) 2.50 - 107 kJ/m²
1.19 - 50.9 ft-lb/in²
Average value: 9.85 kJ/m² Grade Count:38
3.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.70 kJ/m² Grade Count:14
Izod Impact, Unnotched (ISO) 10.0 - 95.0 kJ/m²
4.76 - 45.2 ft-lb/in²
Average value: 47.8 kJ/m² Grade Count:19
35.0 - 67.0 kJ/m²

@Temperature -30.0 - -30.0 °C
16.7 - 31.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 52.8 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.50 - 10.0 J/cm²
7.14 - 47.6 ft-lb/in²
Average value: 5.14 J/cm² Grade Count:58
1.50 - 7.90 J/cm²

@Temperature -30.0 - -20.0 °C
7.14 - 37.6 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.28 J/cm² Grade Count:29
Charpy Impact, Notched 0.100 - 1.80 J/cm²
0.476 - 8.57 ft-lb/in²
Average value: 0.707 J/cm² Grade Count:60
0.100 - 1.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.476 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.545 J/cm² Grade Count:32
Puncture Energy 1.90 - 1.90 J

@Temperature -30.0 - -30.0 °C
1.40 - 1.40 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.90 J Grade Count:1
1.90 - 1.90 J

@Load <=91.8 kg
1.40 - 1.40 ft-lb

@Load <=202 lb
Average value: 1.90 J Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 17.0 - 82.0 µm/m-°C
9.44 - 45.6 µin/in-°F
Average value: 45.3 µm/m-°C Grade Count:22
CTE, linear, Transverse to Flow 23.0 - 105 µm/m-°C
12.8 - 58.3 µin/in-°F
Average value: 77.6 µm/m-°C Grade Count:12
Thermal Conductivity 0.303 - 0.331 W/m-K
2.10 - 2.30 BTU-in/hr-ft²-°F
Average value: 0.321 W/m-K Grade Count:4
Melting Point 215 - 225 °C
419 - 437 °F
Average value: 221 °C Grade Count:62
Maximum Service Temperature, Air 80.0 - 200 °C
176 - 392 °F
Average value: 124 °C Grade Count:8
Hot Ball Pressure Test 123 - 127 °C
253 - 261 °F
Average value: 125 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 130 - 245 °C
266 - 473 °F
Average value: 208 °C Grade Count:60
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 230 °C
158 - 446 °F
Average value: 191 °C Grade Count:115
Vicat Softening Point 195 - 250 °C
383 - 482 °F
Average value: 208 °C Grade Count:57
UL RTI, Electrical 65.0 - 130 °C
149 - 266 °F
Average value: 89.2 °C Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 1.00e+17 ohm-cm
1.00e+12 - 1.00e+17 ohm-cm
Average value: 5.95e+15 ohm-cm Grade Count:52
Surface Resistance 1.00e+8 - 8.00e+15 ohm
1.00e+8 - 8.00e+15 ohm
Average value: 8.06e+14 ohm Grade Count:38
Dielectric Constant 2.90 - 10.0
2.90 - 10.0
Average value: 3.97 Grade Count:20
Dielectric Strength 11.0 - 70.0 kV/mm
280 - 1780 kV/in
Average value: 27.9 kV/mm Grade Count:55
Dissipation Factor 0.00570 - 0.300
0.00570 - 0.300
Average value: 0.0439 Grade Count:16
Comparative Tracking Index 200 - 600 V
200 - 600 V
Average value: 473 V Grade Count:65