Polymer Property : Charpy Impact, Notched = 0.230 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.230 - 3.48 J/cm²
1.09 - 16.6 ft-lb/in²
Average value: 1.74 J/cm² Grade Count:3
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.230 - 2.00 J/cm²
1.09 - 9.52 ft-lb/in²
Average value: 0.820 J/cm² Grade Count:50
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact, Notched 0.230 - 1.80 J/cm²
1.09 - 8.57 ft-lb/in²
Average value: 0.703 J/cm² Grade Count:50
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Charpy Impact, Notched 0.230 J/cm²

@Temperature -23.0 °C
1.09 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Global PP-1100-RC Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation.
Charpy Impact, Notched 0.230 J/cm²

@Temperature 23.0 °C
1.09 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
IRPC Polimaxx Polene 1111R Polypropylene Homopolymer
CHARACTERISTICS: EXCELLENT HIGH STIFFNESS, HEAT STABILITY, HIGH FLOW CONTAIN LONG TERM HEAT AGING ADDITIVE APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, COFFEE MAKER, HAIR DRYER
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
ISO 179/1eA
Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant
Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat sta..
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
ISO 179
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
Plain Cast Resin
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in..
Charpy Impact, Notched 0.230 J/cm²
1.09 ft-lb/in²
Plain Cast Resin
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..