Polymer Property : Linear Mold Shrinkage = 0.00281 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00281 - 0.00900 cm/cm
0.00281 - 0.00900 in/in
Average value: 0.00522 cm/cm Grade Count:21
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.00281 cm/cm
0.00281 in/in
ASTM D955
Plenco 08225 Polyester BMC, Compression Molded
PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert..
Linear Mold Shrinkage 0.00281 cm/cm
0.00281 in/in
ASTM D955
Plenco 3509 Phenolic, Granular, Compression Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..