Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.000200 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000200 - 0.00900 cm/cm
0.000200 - 0.00900 in/in
Average value: 0.00341 cm/cm Grade Count:110
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.000200 - 0.0100 cm/cm
0.000200 - 0.0100 in/in
Average value: 0.00308 cm/cm Grade Count:21
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Linear Mold Shrinkage 0.000200 - 0.00200 cm/cm
0.000200 - 0.00200 in/in
Average value: 0.00110 cm/cm Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Linear Mold Shrinkage 0.000200 - 0.00400 cm/cm
0.000200 - 0.00400 in/in
Average value: 0.000985 cm/cm Grade Count:19
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Linear Mold Shrinkage 0.000200 - 0.0350 cm/cm
0.000200 - 0.0350 in/in
Average value: 0.00317 cm/cm Grade Count:150
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Linear Mold Shrinkage 0.000200 - 0.0350 cm/cm
0.000200 - 0.0350 in/in
Average value: 0.00376 cm/cm Grade Count:47
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.000200 - 0.0150 cm/cm
0.000200 - 0.0150 in/in
Average value: 0.00252 cm/cm Grade Count:28
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Linear Mold Shrinkage 0.000200 - 0.0160 cm/cm
0.000200 - 0.0160 in/in
Average value: 0.00278 cm/cm Grade Count:82
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage 0.000200 - 0.0200 cm/cm
0.000200 - 0.0200 in/in
Average value: 0.00679 cm/cm Grade Count:284
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Linear Mold Shrinkage 0.000200 - 0.00800 cm/cm
0.000200 - 0.00800 in/in
Average value: 0.00255 cm/cm Grade Count:21
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.000200 - 0.00700 cm/cm
0.000200 - 0.00700 in/in
Average value: 0.00211 cm/cm Grade Count:34
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved