Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | ASTM D955 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00400 cm/cm | 0.00400 in/in | ASTM D955 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00400 cm/cm | 0.00400 in/in | Average value: 0.00400 cm/cm Grade Count:4 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00583 cm/cm Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 1499 P X 125056 B Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.17 mm |
0.00400 - 0.00800 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1002 TFE 15 Z Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Average value: 0.00450 cm/cm Grade Count:4 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00580 cm/cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0130 cm/cm | 0.00400 - 0.0130 in/in | Average value: 0.00719 cm/cm Grade Count:24 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |