Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | ASTM D955 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00400 cm/cm | 0.00400 in/in | ASTM D955 |
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00400 - 0.0100 cm/cm | 0.00400 - 0.0100 in/in | Average value: 0.00636 cm/cm Grade Count:21 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2500 A TFE 13 SI 2 Polycarbonate/ABS Alloy (PC/ABS) PTFE Lubricated - Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron TIM 300 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.0140 cm/cm | 0.00400 - 0.0140 in/in | Average value: 0.00857 cm/cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm @Temperature 80.0 - 80.0 °C |
0.00400 - 0.00700 in/in @Temperature 176 - 176 °F |
Average value: 0.00567 cm/cm Grade Count:3 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Average value: 0.00450 cm/cm Grade Count:4 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00580 cm/cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0130 cm/cm | 0.00400 - 0.0130 in/in | Average value: 0.00840 cm/cm Grade Count:25 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade High Flow, Medium ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00600 cm/cm | 0.00400 - 0.00600 in/in | ASTM D955 |
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |