RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer RheTech Products
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
23/23°C; ASTM D792
Filler Content 40 %
40 %
ASTM D5630
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
Flexural Modulus 3.62 GPa
525 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
260 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
Middle Barrel Temperature 216 - 243 °C
420 - 470 °F
Front Barrel Temperature 221 - 249 °C
430 - 480 °F
Nozzle Temperature 227 - 238 °C
440 - 460 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
Dry Time 1 - 2 hour
1 - 2 hour
Moisture Content <= 0.050 %
<= 0.050 %
Recommended
Injection Pressure 2.76 - 10.3 MPa
400 - 1500 psi
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi