| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural
Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 193 - 243 °C | 379 - 469 °F | |
|
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav..
|
|||
| Middle Barrel Temperature | 193 - 243 °C | 379 - 469 °F | |
|
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over..
|
|||
| Middle Barrel Temperature | 227 - 243 °C | 440 - 470 °F | |
|
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||