Processing Properties Metric English Comments
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
441 - 460 °F
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re..
Nozzle Temperature 227 - 238 °C
441 - 460 °F
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu..
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White
Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 210 - 238 °C
410 - 460 °F
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Nozzle Temperature 210 - 238 °C
410 - 460 °F
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Nozzle Temperature 216 - 238 °C
420 - 460 °F
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact
High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol..
Nozzle Temperature 210 - 238 °C
410 - 460 °F
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Nozzle Temperature 210 - 238 °C
410 - 460 °F
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 200 - 238 °C
392 - 460 °F
Average value: 226 °C Grade Count:28
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Nozzle Temperature 227 - 238 °C
440 - 460 °F
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black