| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 210 °C | 410 °F | |
|
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural
Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | Feed Zone |
|
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane
(discontinued **)
Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties and excellent hyrdrolysis resistance...
|
|||
| Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Start Point: 215°C |
|
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation ..
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Start Point: 230°C |
|
Kingfa MAC-301 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Uses include electric/electronic parts.
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
|
|||
| Rear Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
|
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled
For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | C1 |
|
Kostat E-2001 Conductive PP Compound
KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200..
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Unitika AX-1500 Dry
AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in..
|
|||
| Rear Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Unitika AXG-1500-300 Conditioned
Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd.
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | Injection |
|
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
|
|||
| Rear Barrel Temperature | 210 - 216 °C | 410 - 421 °F | |
|
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer
Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer ..
|
|||
| Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin
10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
|
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin
30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | Injection |
|
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | |
|
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
|
|||
| Rear Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 210 °C | 410 °F | Injection |
|
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.
|
|||