| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural
Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural
Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 293 °C | 440 - 560 °F | |
|
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
|
|||
| Nozzle Temperature | 227 °C | 441 °F | |
|
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane
Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided..
|
|||
| Nozzle Temperature | 227 °C | 441 °F | |
|
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic
Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol
|
|||
| Nozzle Temperature | 227 - 277 °C | 440 - 530 °F | |
|
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer
Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s..
|
|||
| Nozzle Temperature | 227 - 277 °C | 440 - 530 °F | |
|
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer
Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for ..
|
|||
| Nozzle Temperature | 227 - 277 °C | 440 - 530 °F | |
|
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
|
|||
| Nozzle Temperature | 227 - 277 °C | 441 - 531 °F | |
|
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer
Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer ..
|
|||
| Nozzle Temperature | 227 - 249 °C | 440 - 480 °F | |
|
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer
DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a..
|
|||
| Nozzle Temperature | 227 - 249 °C | 440 - 480 °F | |
|
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a..
|
|||
| Nozzle Temperature | 227 - 293 °C | 440 - 560 °F | Average value: 254 °C Grade Count:5 |
|
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||