| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural
Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White
Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||