| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 441 - 460 °F | |
|
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re..
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural
Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 200 - 238 °C | 392 - 460 °F | Average value: 219 °C Grade Count:6 |
|
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
|
|||
| Nozzle Temperature | 216 - 238 °C | 420 - 460 °F | |
|
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
|
|||
| Nozzle Temperature | 216 - 238 °C | 420 - 460 °F | |
|
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
|
|||
| Nozzle Temperature | 216 - 238 °C | 420 - 460 °F | |
|
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black
For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add..
|
|||
| Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
|
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
|
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 200 - 238 °C | 392 - 460 °F | Average value: 226 °C Grade Count:28 |
|
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
|
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 218 - 238 °C | 425 - 460 °F | Average value: 229 °C Grade Count:5 |
|
Overview of materials for Polypropylene with 40% Mica Filler