RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer RheTech Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
23/23°C; ASTM D792
Filler Content 33 %
33 %
ASTM D5630
Linear Mold Shrinkage 0.0105 cm/cm
0.0105 in/in
ASTM D955
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 15.9 MPa
2300 psi
2 in/min; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.33 J/cm

@Temperature 23.0 °C
2.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 18.2 J
13.4 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
Nozzle Temperature 221 - 232 °C
430 - 450 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
Dry Time 1 - 2 hour
1 - 2 hour
Moisture Content <= 0.050 %
<= 0.050 %
Recommended
Injection Pressure 2.76 - 10.3 MPa
400 - 1500 psi
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Users viewing this material also viewed the following: