| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1563 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1566L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1766B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1900-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2156 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2260-R1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2354 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1357A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1389E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-1393B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2955 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
|
Teknor Apex Monprene® MP-2830 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||