Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.50 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.33 J/cm

@Temperature 23.0 °C
2.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.33 J/cm

@Temperature 23.0 °C
2.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Omni Plastics OmniTech™ PC GR40 Glass Reinforced Polycarbonate
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (Cond)
Information provided by Ravago.
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
M. Holland Company CP503 Polypropylene Impact Copolymer
Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding
Izod Impact, Notched 1.33 J/cm

@Thickness 3.20 mm
2.50 ft-lb/in

@Thickness 0.126 in
ASTM D256
KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS
Key features: Translucent Injection. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resista..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Elastoblend® PA6 GF20 IM2 BK 20% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF40 L BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Total PSI 935E Polystyrene
Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Ecomass® 3620BX18 5% Borated Polyethylene (HDPE)
5% Borated Polyethylene (HDPE), Product Form - Pellets, No Pre-Drying RequiredProcessing Method: Injection Molding, Compression MoldingNeutron Shielding ApplicationsInformation provided by Technica..
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
Method A, Injection Molded, 0.125 in bars, 73°F; ASTM D648
PolyOne Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp  (discontinued **)
Information provided by PolyOne™ Corporation
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C..
Copyright © lookpolymers.com All Rights Reserved