Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Polymax® Maxelast® D6770 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D 792 |
Karina TR-700-35/1 Ivory PVC Compound PVC compound with addition of nitrile rubber, recommended for injection of solesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D 792 |
Karina 702-DA-18/406-BZ-AS Gray PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Momentive Performance Materials Addisilâ„¢ 472 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Momentive Performance Materials RTV6424 Heat-Curing Silicone Adhesive, White RTV6424, RTV6445, and TSE322 silicone adhesives are one-component heat curable silicone adhesive sealants which will bond to many substrates without a primer and which will creep rapidly at elevated.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Spartech 1462-51 NA43 PVC and Alloy Products for Footwear Used for long life solingInformation provided by Spartech |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3201-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Teknor Apex APEX® 90-A471R-6-NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | DIN 53479 |
Lubrizol ESTANE® T4057 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE DescriptionPOLYBATCH® 40442 is a light blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40442 is typical.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | Mixed |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Lubrizol Estane® CS185A Thermoplastic Polyurethane Type: Estane® CS185A is a Shore 85A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
ELASTO UK Dryflex® 602850S SEBS Based Material, Filled Qualities, 85A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Colorite Polymers Vinylbond 95-950-55 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
E-Polymers TEKAMID® HG10L 10% Glass Fiber Reinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Specific Gravity | 1.17 - 1.21 g/cc | 1.17 - 1.21 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom CE-553165 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | Molded plaque; ISO 2577 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Cheng Yu Plastic A707G25 SAN, 25% Glass Fiber |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Colorite Polymers 5512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Specific Gravity | 1.17 - 1.21 g/cc | 1.17 - 1.21 g/cc | ASTM D-792 |
Axiall 14700 Wire & Cable Flexible PVC Clear, flexible PVC compound recommended for SPT applications. Maximum service temperature rating of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | Part A; TM R050-16 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |