| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
|
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black
Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
|
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo..
|
|||
| Front Barrel Temperature | 216 - 235 °C | 420 - 455 °F | |
|
Ravago Manufacturing Americas Hylac® GP55 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Front Barrel Temperature | 216 - 235 °C | 420 - 455 °F | |
|
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
|
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
|
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel
Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
|
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
|
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app..
|
|||
| Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
|
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq..
|
|||
| Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
|
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha..
|
|||
| Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
|
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
|
|||
| Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
|
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
|
|||
| Front Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,..
|
|||
| Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
|
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app..
|
|||
| Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
|
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
|
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..
|
|||
| Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
|
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||