Processing Properties Metric English Comments
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Front Barrel Temperature 216 - 260 °C
420 - 500 °F
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black
Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black
Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo..
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Ravago Manufacturing Americas Hylac® GP55 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Ravago Manufacturing Americas Hylac® HF96 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 216 °C
420 °F
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In..
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel
Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas..
Front Barrel Temperature 216 °C
420 °F
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin  (Unverified Data**)
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Front Barrel Temperature 216 - 227 °C
420 - 440 °F
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have an excellent soft t..
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Front Barrel Temperature 216 - 243 °C
420 - 470 °F
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.