Overview of materials for Nylon 6, 20% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Overview of materials for Nylon 6, 20% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.14 - 1.67 g/cc
0.0412 - 0.0603 lb/in³
Average value: 1.27 g/cc Grade Count:363
1.07 - 1.07 g/cc
<br>@Temperature 270 - 270 °C
0.0387 - 0.0387 lb/in³
<br>@Temperature 518 - 518 °F
Average value: 1.07 g/cc Grade Count:1
Filler Content 15.0 - 25.0 %
15.0 - 25.0 %
Average value: 17.8 % Grade Count:75
Water Absorption 0.150 - 9.50 %
0.150 - 9.50 %
Average value: 3.65 % Grade Count:160
2.40 - 2.90 %
<br>@Temperature 70.0 - 70.0 °C
2.40 - 2.90 %
<br>@Temperature 158 - 158 °F
Average value: 2.65 % Grade Count:4
Moisture Absorption at Equilibrium 0.170 - 8.00 %
0.170 - 8.00 %
Average value: 2.40 % Grade Count:104
Water Absorption at Saturation 5.00 - 9.00 %
5.00 - 9.00 %
Average value: 7.59 % Grade Count:39
Viscosity 300000 - 350000 cP
<br>@Temperature 280 - 280 °C
300000 - 350000 cP
<br>@Temperature 536 - 536 °F
Average value: 325000 cP Grade Count:2
300000 - 350000 cP
<br>@Shear Rate 1000 - 1000 1/s
300000 - 350000 cP
<br>@Shear Rate 1000 - 1000 1/s
Average value: 325000 cP Grade Count:2
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 148 cm³/g Grade Count:8
Maximum Moisture Content 0.100
0.100
Average value: 0.100 Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00511 cm/cm Grade Count:287
0.00400 - 0.00700 cm/cm
<br>@Temperature 80.0 - 80.0 °C
0.00400 - 0.00700 in/in
<br>@Temperature 176 - 176 °F
Average value: 0.00567 cm/cm Grade Count:3
Linear Mold Shrinkage, Transverse 0.00160 - 0.0197 cm/cm
0.00160 - 0.0197 in/in
Average value: 0.00903 cm/cm Grade Count:127
0.00800 - 0.0100 cm/cm
<br>@Temperature 80.0 - 80.0 °C
0.00800 - 0.0100 in/in
<br>@Temperature 176 - 176 °F
Average value: 0.00867 cm/cm Grade Count:3
Melt Flow 1.00 - 100 g/10 min
1.00 - 100 g/10 min
Average value: 26.4 g/10 min Grade Count:55
Spiral Flow 55.0 - 100 cm
21.7 - 39.4 in
Average value: 82.4 cm Grade Count:16
Mechanical Properties Metric English Comments
Hardness, Rockwell L 110 - 123
110 - 123
Average value: 117 Grade Count:4
Hardness, Rockwell M 80.0 - 100
80.0 - 100
Average value: 91.1 Grade Count:9
Hardness, Rockwell R 90.0 - 122
90.0 - 122
Average value: 117 Grade Count:61
Hardness, Shore D 73.0 - 91.0
73.0 - 91.0
Average value: 79.5 Grade Count:11
Ball Indentation Hardness 70.0 - 200 MPa
10200 - 29000 psi
Average value: 155 MPa Grade Count:31
Tensile Strength, Ultimate 13.8 - 180 MPa
2000 - 26100 psi
Average value: 105 MPa Grade Count:277
10.0 - 163 MPa
<br>@Temperature -40.0 - 150 °C
1450 - 23600 psi
<br>@Temperature -40.0 - 302 °F
Average value: 69.4 MPa Grade Count:8
60.0 - 75.0 MPa
<br>@Temperature 130 - 175 °C
8700 - 10900 psi
<br>@Temperature 266 - 347 °F
Average value: 69.4 MPa Grade Count:2
60.0 - 75.0 MPa
<br>@Time 1.80e+7 - 7.20e+7 sec
8700 - 10900 psi
<br>@Time 5000 - 20000 hour
Average value: 69.4 MPa Grade Count:2
Tensile Strength, Yield 60.0 - 195 MPa
8700 - 28300 psi
Average value: 114 MPa Grade Count:91
53.0 - 53.0 MPa
<br>@Temperature 80.0 - 80.0 °C
7690 - 7690 psi
<br>@Temperature 176 - 176 °F
Average value: 53.0 MPa Grade Count:1
Elongation at Break 1.00 - 28.0 %
1.00 - 28.0 %
Average value: 5.10 % Grade Count:316
1.20 - 15.0 %
<br>@Temperature -40.0 - 150 °C
1.20 - 15.0 %
<br>@Temperature -40.0 - 302 °F
Average value: 5.57 % Grade Count:4
Elongation at Yield 2.00 - 18.0 %
2.00 - 18.0 %
Average value: 6.31 % Grade Count:27
1.70 - 8.60 %
<br>@Temperature 80.0 - 150 °C
1.70 - 8.60 %
<br>@Temperature 176 - 302 °F
Average value: 3.76 % Grade Count:3
Modulus of Elasticity 0.0630 - 14.3 GPa
9.14 - 2070 ksi
Average value: 5.31 GPa Grade Count:238
0.886 - 6.50 GPa
<br>@Temperature -20.0 - 200 °C
129 - 943 ksi
<br>@Temperature -4.00 - 392 °F
Average value: 3.09 GPa Grade Count:4
Flexural Yield Strength 55.0 - 300 MPa
7980 - 43500 psi
Average value: 167 MPa Grade Count:233
45.0 - 240 MPa
<br>@Temperature -40.0 - 90.0 °C
6530 - 34800 psi
<br>@Temperature -40.0 - 194 °F
Average value: 116 MPa Grade Count:4
Flexural Modulus 1.50 - 10.3 GPa
218 - 1490 ksi
Average value: 5.11 GPa Grade Count:252
1.70 - 8.00 GPa
<br>@Temperature -40.0 - 120 °C
247 - 1160 ksi
<br>@Temperature -40.0 - 248 °F
Average value: 3.83 GPa Grade Count:5
Compressive Yield Strength 103 - 145 MPa
14900 - 21000 psi
Average value: 127 MPa Grade Count:9
Poissons Ratio 0.350 - 0.380
0.350 - 0.380
Average value: 0.356 Grade Count:5
Shear Modulus 1.37 - 2.60 GPa
199 - 377 ksi
Average value: 2.16 GPa Grade Count:6
>= 0.0108 GPa
<br>@Temperature -100 - 200 °C
>= 1.57 ksi
<br>@Temperature -148 - 392 °F
Average value: 1.02 GPa Grade Count:2
Izod Impact, Notched 0.300 - 2.51 J/cm
0.562 - 4.70 ft-lb/in
Average value: 0.896 J/cm Grade Count:124
0.300 - 0.600 J/cm
<br>@Temperature -40.0 - -20.0 °C
0.562 - 1.12 ft-lb/in
<br>@Temperature -40.0 - -4.00 °F
Average value: 0.752 J/cm Grade Count:4
0.588399 - 1.49492 J/cm
<br>@Temperature -30.0 - -20.0 °C
1.10231 - 2.80060 ft-lb/in
<br>@Temperature -22.0 - -4.00 °F
Average value: 0.752 J/cm Grade Count:5
0.588399 - 1.49492 J/cm
<br>@Thickness 3.17 - 6.40 mm
1.10231 - 2.80060 ft-lb/in
<br>@Thickness 0.125 - 0.252 in
Average value: 0.752 J/cm Grade Count:5
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 6.43 J/cm Grade Count:22
Izod Impact, Notched (ISO) 4.00 - 64.0 kJ/m²
1.90 - 30.5 ft-lb/in²
Average value: 11.1 kJ/m² Grade Count:73
3.00 - 13.0 kJ/m²
<br>@Temperature -40.0 - -20.0 °C
1.43 - 6.19 ft-lb/in²
<br>@Temperature -40.0 - -4.00 °F
Average value: 7.82 kJ/m² Grade Count:32
Izod Impact, Unnotched (ISO) 10.0 - 90.0 kJ/m²
4.76 - 42.8 ft-lb/in²
Average value: 54.4 kJ/m² Grade Count:29
30.0 - 79.0 kJ/m²
<br>@Temperature -40.0 - -30.0 °C
14.3 - 37.6 ft-lb/in²
<br>@Temperature -40.0 - -22.0 °F
Average value: 45.7 kJ/m² Grade Count:22
Charpy Impact Unnotched 1.50 J/cm² - NB
7.14 ft-lb/in² - NB
Average value: 6.09 J/cm² Grade Count:181
1.50 J/cm² - NB
<br>@Temperature -40.0 - 30.0 °C
7.14 ft-lb/in² - NB
<br>@Temperature -40.0 - 86.0 °F
Average value: 4.74 J/cm² Grade Count:124