| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature -30.0 °C
|
1.90
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature -30.0 °C
|
1.90
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML3729 PC
Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO 180/1A |
|
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | Low Temp; DIN 53453 |
|
Ineos Nova S-5400 High Impact Compact Polystyrene
(discontinued **)
Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
|
|||
| Izod Impact, Notched (ISO) | 4.00 - 67.0 kJ/m² | 1.90 - 31.9 ft-lb/in² | Average value: 22.5 kJ/m² Grade Count:30 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
|
|||
| Izod Impact, Notched (ISO) |
4.00
-
10.0
kJ/m² <br>@Temperature -30.0 - 0.000 °C
|
1.90
-
4.76
ft-lb/in² <br>@Temperature -22.0 - 32.0 °F
|
Average value: 6.80 kJ/m² Grade Count:9 |
|
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
|
|||
| Izod Impact, Notched (ISO) |
4.00
-
8.00
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
1.90
-
3.81
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 5.67 kJ/m² Grade Count:3 |
|
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s).
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature 23.0 °C
|
1.90
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific)
LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM DU319 PEI
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO Test |
|
Styrolution Styrolux 684D SBC
Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO 180/1A |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature -30.0 °C
|
1.90
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East)
LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP WF0049XP PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WF0049XP is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature 23.0 °C
|
1.90
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Polyram PlusTek PB340S4 Nylon 6 for Injection Molding, 20% Glass-Beads Reinforced
20% Glass-beads reinforced, Nylon 6 for injection molding applications.Information provided by Polyram.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO 180/1A |
|
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)<
Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance ..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded
Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² <br>@Temperature -40.0 °C
|
1.90
ft-lb/in² <br>@Temperature -40.0 °F
|
Brittle break; ISO 180 |
|
Brueggemann Chemical Nyrim® 1000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||