Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.00100 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
ASTM D955
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00100 - 0.00550 cm/cm
0.00100 - 0.00550 in/in
Average value: 0.00266 cm/cm Grade Count:23
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00250 cm/cm Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00700 cm/cm Grade Count:14
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00332 cm/cm Grade Count:111
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cm
0.00100 - 0.00700 in/in
Average value: 0.00443 cm/cm Grade Count:7
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00514 cm/cm Grade Count:11
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm
0.00100 - 0.00600 in/in
Average value: 0.00468 cm/cm Grade Count:11
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cm
0.00100 - 0.00700 in/in
Average value: 0.00342 cm/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Linear Mold Shrinkage 0.00100 - 0.0340 cm/cm
0.00100 - 0.0340 in/in
Average value: 0.0148 cm/cm Grade Count:214
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00494 cm/cm Grade Count:152
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.0118 cm/cm Grade Count:49
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm
0.00100 - 0.00600 in/in
Average value: 0.00332 cm/cm Grade Count:17
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00333 cm/cm Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm
0.00100 - 0.0250 in/in
Average value: 0.0131 cm/cm Grade Count:17
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00469 cm/cm Grade Count:144
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cm
0.00100 - 0.00700 in/in
Average value: 0.00290 cm/cm Grade Count:26
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00243 cm/cm Grade Count:5
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00204 cm/cm Grade Count:12
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00624 cm/cm Grade Count:373
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm
0.00100 - 0.00600 in/in
Average value: 0.00313 cm/cm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage 0.00100 - 0.0150 cm/cm
0.00100 - 0.0150 in/in
Average value: 0.00625 cm/cm Grade Count:9
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00240 cm/cm Grade Count:5
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00525 cm/cm Grade Count:12
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00341 cm/cm Grade Count:33
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm
0.00100 - 0.0250 in/in
Average value: 0.0122 cm/cm Grade Count:14
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00629 cm/cm Grade Count:115
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00511 cm/cm Grade Count:287
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm
0.00100 - 0.00600 in/in
Average value: 0.00376 cm/cm Grade Count:4
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..