| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled |
| Manufacturer | LG Chemical |
| Trade Name | LUMID |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Yield | 157 MPa @Thickness 3.20 mm |
22800 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
| Elongation at Break | 4.0 % @Thickness 3.20 mm |
4.0 % @Thickness 0.126 in |
5mm/min; ASTM D638 |
| Flexural Yield Strength | 221 MPa @Thickness 6.40 mm |
32000 psi @Thickness 0.252 in |
3mm/min; ASTM D790 |
| Flexural Modulus | 6.86 GPa @Thickness 6.40 mm |
996 ksi @Thickness 0.252 in |
3mm/min; ASTM D790 |
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM D696 |
| Melting Point | 260 °C | 500 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °C @Thickness 6.40 mm |
500 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C @Thickness 6.40 mm |
473 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
| 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 110 °C @Thickness >=0.750 mm |
230 °F @Thickness >=0.0295 in |
|
| 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
||
| 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
| 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | HB @Thickness >=0.750 mm |
HB @Thickness >=0.0295 in |
|
| HB @Thickness >=1.50 mm |
HB @Thickness >=0.0591 in |
||
| HB @Thickness >=3.00 mm |
HB @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 4.0 @Frequency 1.00e+6 Hz |
4.0 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 25.0 kV/mm @Thickness 1.00 mm |
635 kV/in @Thickness 0.0394 in |
ASTM D149 |
| Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
| 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
||
| 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
| >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
||
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 265 - 275 °C | 509 - 527 °F | Injection Molding |
| Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
| Front Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |