Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.010 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ASTM D955
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® LUX1619 PC
Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® LUX2619 PC
Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® PPC4701 PPC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 3.17 mm
0.0070 - 0.010 in/in

@Thickness 0.125 in
ASTM D955
Ravago Manufacturing Americas Enviramid™ N2340MHL BK Post Consumer Recycle Nylon 6, 40% Mineral Filled
Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.0040 - 0.010 cm/cm

@Thickness 3.20 mm
0.0040 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUCON PN9008 PPS+MF+GF
Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212..
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm

@Thickness 3.20 mm
0.0050 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact
Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm

@Thickness 3.20 mm
0.0050 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact
Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm

@Thickness 3.20 mm
0.0050 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 3.20 mm
0.0070 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0030 - 0.010 cm/cm

@Thickness 3.20 mm
0.0030 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP2306FB PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0030 - 0.010 cm/cm

@Thickness 3.20 mm
0.0030 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP2306FC PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0030 - 0.010 cm/cm

@Thickness 3.20 mm
0.0030 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP2306FS PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem..
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 3.20 mm
0.0070 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® TE5000LZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide..
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 3.20 mm
0.0070 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® TE5000SZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 3.20 mm
0.0070 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL GP3400S PP+MF40%
Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica..
Linear Mold Shrinkage, Flow 0.0090 - 0.010 cm/cm

@Thickness 3.20 mm
0.0090 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
LATI Laticonther 83 CP/85 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Time 86400 sec
0.0070 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0049F PC
LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding...
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific)
Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0025 - 0.010 cm/cm

@Thickness 3.20 mm
0.0025 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® XP-2140C PPS
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Time 86400 sec
0.0070 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66
LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm

@Thickness 4.00 mm
0.0070 - 0.010 in/in

@Thickness 0.157 in
E2P method
Eurostar Staramide 6 80E7 PA6, Injection Molded
Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm

@Thickness 4.00 mm
0.0050 - 0.010 in/in

@Thickness 0.157 in
E2P method
Eurostar Starpylen HU 30BF4 PP, 30% Bamboo Fiber Filled, Injection Molding
Starpylen HU30BF4 is a 30% Bamboo Fiber Reinforced Polypropylene Injection Molding Resin (also known as HU30BF4) (PRELIMINARY DATASHEET)Information provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
on Tensile Bar; E2P method
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.