Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**) Zytel® FE270050 BK099 is a 30% glass reinforced, polyamide 66 resin for gas and water assisted injection molding.Information provided by DuPont |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | Injection Molding |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Recommended |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latilub 62-01M G/30 PA6, 30% Glass Fiber Reinforced Self-lubricating product based on Polyamide 6 (PA6). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Corbion Purac Blend A High Heat Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Data is for samples produced from Puralact L and D lactide monomers; Purac also produces .. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
CP-Polymer-Technik Wellamid® 6000 CF 30 HWCP 30% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 5 HWCP 5% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural Information provided by Eurotec® |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
E-Polymers TEKALOY® G70NHT Non Halogen Flame Retardant Impact Resistance PC/ABS Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |