Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 225 - 280 °C | 437 - 536 °F | Average value: 246 °C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | Average value: 263 °C Grade Count:12 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Nozzle Temperature | 235 - 280 °C | 455 - 536 °F | Average value: 263 °C Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |