| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Packaging XPL189 Amber 1505 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio..
|
|||
| Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | |
|
Raschig Group PiMC 1253 Highly flame retardant
This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible SL9994 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible XV3845 Polyvinyl Chloride, Flexible (PVC, Flexible)
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard..
|
|||
| Specific Gravity |
1.30
g/cc <br>@Temperature 23.0 °C
|
1.30
g/cc <br>@Temperature 73.4 °F
|
ISO 1183 |
|
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced
Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
|
|||
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
|
Gromax PBT 1100-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications
Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf..
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
|
Karina 851D48/1-A-IS-LMP Black PVC Compound
Heavy metal free PVC compound class 70C (ST1), recommended for electrical flexible cables jacketing. Also suitable for injection of plug.Information provided by Karina Indústria e Comércio de..
|
|||
| Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
|
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films, laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105-7709/RD PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
|
Sylvin Technologies 8925-75 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific)
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® VB-4921 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Teknor Apex APEX® 80862-F Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Cheng Yu Plastic FR200GV20 Flame Retardant Nylon 66, 20% Glass Fiber |
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
Cheng Yu Plastic FRCV200 Flame Retardant Nylon 66, 30% Mineral Reinforced |
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Yellow 26787V Concentrate Based In LDPE
DescriptionPOLYBATCH® 2787V is a yellow color concentrate with added process aid based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBAT..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
|
|||
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
|
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific)
Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
|
|||