Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable Y66A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | <= 1.30 g/cc | <= 1.30 g/cc | ASTM D792, A |
S&E Specialty Polymers XP23-566-1 PVC Description: PVC weatherable, integral colored, filledApplication: Low gloss lift gate molding compound which meets Chrysler MSDC 543.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.30 - 2.00 g/cc | 1.30 - 2.00 g/cc | |
Nanocyl NANOCYL™ NC7000 Thin Multi-Wall Carbon Nanotubes NANOCYL™ NC7000 Series, thin multi-wall carbon nanotubes, are produced via the catalytic carbon vapor deposition (CCVD) process.These carbon nanotubes are unique and prized world-wide because their.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Specific Gravity | 1.30 g/cc @Temperature 23.0 °C |
1.30 g/cc @Temperature 73.4 °F |
ISO 1183 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Specific Gravity | 1.30 - 1.35 g/cc @Thickness 1.57 mm |
1.30 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP600 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062".. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Silberline 4-Allâ„¢ E2776AR The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Sylvin Technologies 6046 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 26787V Concentrate Based In LDPE DescriptionPOLYBATCH® 2787V is a yellow color concentrate with added process aid based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBAT.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | IEC 1212-2 8.1 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom BD-330699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |
|||
Specific Gravity | 1.30 g/cc @Temperature 25.0 °C |
1.30 g/cc @Temperature 77.0 °F |
|
Dow Corning 5-8601 FLUOROSILICONE LSR, KIT Fluorosilicone rubber designed for liquid injection moldingInformation provided by Dow Corning |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | mixed, uncured |
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | Base |
ACC QM 262F QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 262F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced Information provided by Ravago. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 26787V Concentrate Based In LDPE DescriptionPOLYBATCH® 2787V is a yellow color concentrate with added process aid based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBAT.. |