Manufacturer : Addiplast > Category : Polypropylene (PP) Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Addiplast Addilene H 140 Polypropylene Homopolymer Polypropylene, Extrusion Grade Addilene
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Polypropylene Glass Bead Filled Addilene
Addiplast Addilene H 211 V20 Polypropylene Homopolymer Polypropylene, Glass Reinforced, Impact Modified Addilene
Addiplast Addilene H 220 M40 Polypropylene Homopolymer Polypropylene, Mineral Reinforced Addilene
Addiplast Addilene H 220 T20 Polypropylene Homopolymer Polypropylene, Mineral Reinforced Addilene
Addiplast Addilene H 242 M40 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 410 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 490 S Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 520 M40 Polypropylene Homopolymer Polypropylene, Mineral Reinforced Addilene
Addiplast Addilene H 520 T40 Polypropylene Homopolymer Polypropylene, Mineral Reinforced Addilene
Addiplast Addilene H 526 N30 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 532 N30 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 542 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 560 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 652 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene J 110 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 120 M10 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 120 M20 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 220 M20 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 310 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 370 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 380 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 420 K24 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene J 490 S Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene J 510 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 520 M20 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 520 M40 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 522 K20 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 522 M20 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 522 N30 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene PMD 50213 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50215 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50218 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene PMD 50245 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene PMD 50258 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 420 K24 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 490 M40F Flame Retardant Polypropylene, 40% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 511 V30 Polypropylene Homopolymer Polypropylene, Glass Reinforced, Impact Modified Addilene
Addiplast Addilene J 220 M40 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene J 430 N30 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 470 ST14 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled Polypropylene, Flame Retardant Addilene
Addiplast Addilene J 520 T30 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene J 683 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50271 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene PMD 50284 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50306 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene H 210 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 442 M30 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene H 462 M20 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Polypropylene, Molded Addilene
Addiplast Addilene J 326 V30 Polypropylene Copolymer Polypropylene Copolymer Addilene
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene Polypropylene, Flame Retardant Addilene