| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
| Manufacturer | Addiplast |
| Trade Name | Addilene |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addilene PMD 50291 Flame Retardant Polypropylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183/A |
| Melt Flow | 16 g/10 min | 16 g/10 min | ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | Conditioned; ISO 868 |
| Tensile Strength at Break | 36.0 MPa | 5220 psi | Conditioned; ISO R 527 |
| Elongation at Break | 3.0 % | 3.0 % | Conditioned; ISO R 527 |
| Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
| Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
| Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | Conditioned; ISO 179/IeU |
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | ISO 75-2/AF |
| Vicat Softening Point | 150 °C | 302 °F | ISO 306/A50 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| Oxygen Index | 22 % | 22 % | ISO 4589 |
| Glow Wire Test | 850 °C | 1560 °F | CEI 60695/2/1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | Conditioned; CEI 60093 |
| Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | Conditioned; CEI 60093 |
| Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |