Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addilene H 532 N30 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene H 532 N30 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Good surface appearanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Melt Flow 18 g/10 min
18 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ISO 868
Tensile Strength at Break 19.0 MPa
2760 psi
ISO R 527
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO R 527
Elongation at Yield 16 %
16 %
ISO R 527
Modulus of Elasticity 2.90 GPa
421 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/IeU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-2/AF
Vicat Softening Point 153 °C
307 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
CEI 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A