Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addilene J 522 N30 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene J 522 N30 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mineral reinforced, improved scratch resistanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength at Break 20.0 MPa
2900 psi
ISO R 527
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO R 527
Elongation at Yield 15 %
15 %
ISO R 527
Modulus of Elasticity 2.50 GPa
363 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/IeU
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ISO 75-2/AF
Vicat Softening Point 152 °C
306 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
CEI 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A
Users viewing this material also viewed the following: