| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer |
| Manufacturer | Addiplast |
| Trade Name | Addilene |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addilene J 310 Polypropylene Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183/A |
| Melt Flow | 6.0 g/10 min | 6.0 g/10 min | ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 66 | 66 | ISO 868 |
| Tensile Strength at Break | 28.0 MPa | 4060 psi | ISO R 527 |
| Tensile Strength, Yield | 32.0 MPa | 4640 psi | ISO R 527 |
| Elongation at Yield | >= 100 % | >= 100 % | ISO R 527 |
| Modulus of Elasticity | 1.00 GPa | 145 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1A |
| Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 52.0 °C | 126 °F | ISO 75-2/AF |
| Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | CEI 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 |
| Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |