Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer LG Chemical
Trade Name LUPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner, mud guard, door trim, garnishElectrical and Electronic: Tail lamp housing, air conditioner housing, fan, socket, washing machine partsIndustrial Parts and Household Appliance:Propeller fan, pulley, container, pump container, pump casing, handle and switch cover of electric jar, fan shroud/supportInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 4.20 GPa
609 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
273 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 220 °C
392 - 428 °F
Middle Barrel Temperature 200 - 230 °C
392 - 446 °F
Front Barrel Temperature 210 - 230 °C
410 - 446 °F
Nozzle Temperature 210 - 240 °C
410 - 464 °F
Melt Temperature 210 - 240 °C
410 - 464 °F
Mold Temperature 40.0 - 90.0 °C
104 - 194 °F
Drying Temperature 70.0 - 90.0 °C
158 - 194 °F
Dry Time 2 - 3 hour
2 - 3 hour
Injection Pressure 29.4 - 118 MPa
4260 - 17100 psi
First
78.45 - 98.07 MPa
11380 - 14220 psi
Second
Back Pressure 0.490 - 3.92 MPa
71.1 - 569 psi
Screw Speed 40 - 60 rpm
40 - 60 rpm
Users viewing this material also viewed the following: