Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable Polycarbonate, 5% Glass Reinforced, Impact Modified, FoamableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 238 - 266 °C | 460 - 510 °F | |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Entec Hylex® P1017FR Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Rear Barrel Temperature | 243 - 266 °C | 470 - 510 °F | |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |