Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hybrid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 3.80 kg,
Temperature 250 °C
20 g/10 min

@Load 8.38 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D638
Flexural Yield Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
73°F, 0.125 in; ASTM D256
Processing Properties Metric English Comments
Rear Barrel Temperature 243 - 266 °C
470 - 510 °F
Middle Barrel Temperature 249 - 271 °C
480 - 520 °F
Front Barrel Temperature 254 - 277 °C
490 - 530 °F
Nozzle Temperature 254 - 271 °C
490 - 520 °F
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Drying Temperature 110 °C
230 °F
Dry Time 4 - 6 hour
4 - 6 hour
Shot Size 50 - 80 %
50 - 80 %
Screw Speed 50 - 80 rpm
50 - 80 rpm
Descriptive Properties Value Comments
Injection Rate Moderate
Users viewing this material also viewed the following: