| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled , Nylon 6, Heat Stabilized |
| Manufacturer | Clariant |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
| Filler Content | 40 % | 40 % | ASTM D2584 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Yield Strength | 124 MPa | 18000 psi | ASTM D790 |
| Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
| Izod Impact, Notched | 0.481 J/cm <br>@Temperature 22.8 °C |
0.900 ft-lb/in <br>@Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 121 °C | 250 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
| Middle Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
| Front Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
| Nozzle Temperature | 254 - 274 °C | 490 - 525 °F | |
| Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
| Mold Temperature | 79.4 - 121 °C | 175 - 250 °F | |
| Dry Time | 2 - 4 hour <br>@Temperature 79.4 °C |
2 - 4 hour <br>@Temperature 175 °F |
to ensure moisture content is less than 0.2% |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 MPa | 50.0 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |