Processing Properties Metric English Comments
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced
Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow
High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-GP1 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized
Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 266 °C
480 - 510 °F
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Rear Barrel Temperature 249 - 254 °C
480 - 490 °F
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved